Both straight grates and grate kilns dry the pellets out in a drying section, then bring the pellets up to a temperature of about 800-900 °C in a preheat zone, then finish the induration process at roughly 1200-1350 °C. The pellets are then cooled to a suitable temperature for transporting to a load out facility.