US3953200A - Nickel extraction process - Google Patents
Twenty grams of low-grade nickel ore, pulverized to about 14 mesh, are charged to a ball mill. One hundred milliliters of ammonia/ammonium salt leach solution are also charged to said ball mill. Grinding is then begun and carried on at room temperatures and atmospheric pressure for a period of about 24 hours.